Saturday, November 4, 2023

Re: [MW:34624] Welder Qualified on Plate can weld Pipe?

Welder qualified on plate can weld 73mm OD and over. Thickness limit will be 2T of plate qualified.

Regards

Pradeep

On Sat, 4 Nov, 2023, 16:07 sachin sunny N, <sachinsunnyn25@gmail.com> wrote:
Dear Experts,

Does a welder qualified on plate can do weld on pipe as per ASME? What is the range for that?

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/eb81cef5-8919-4571-8ada-9222906f059dn%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAAWS%2BE9akfufLtL_JVNNHLNvS5midojgmGGK5EuzGpKsK67ZjA%40mail.gmail.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...