I suppose this is a structural material. Rerolling does not reduce the Material Thickness and it is done to obtain uniform curvature and does not induce any stresses. In structural material, even Flame straightening below 600 deg C is permitted.

Just for a precaution, you can have the L-seam RT tested after rerolling.

Thanks & Regards

J.Gerald Jayakumar




On Wednesday, 27 September, 2023 at 07:22:34 pm IST, RAJESH KUMAR <rajeshkumarbhaskara@gmail.com> wrote:


Dear Expert,

During a site observation, a subcontractor's carbon steel shell (EH36, thickness 40 mm) was found re-rolled due to ovality after 100% of the NDT(UT&MPI) long seam welds. Many stresses come and grain boundaries are stretched after rolling such a thick joint.Any experts please advise.

Standard - DNV-OSC -401
Construction specifications - AWS D1.1
image.png


Thanks & Regards

Rajesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfO5WESSOFt_GNicQH25ffSSuAHHGSSfNkCMp2FRCzLAMQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...