Thursday, September 14, 2023

Re: [MW:34544] Material Inspection Acceptance

What is your plate material specification? 

Material specification always refers to General specification requirements for plate size, dimensions, straightness as well as physical & mechanical properties.

For example if your material is SA 516 then you can find general requirements in SA 20 for all the tolerances and deviations.

Thanks & Regards

K.Dinesh 

Metallurgist





On Thu, Sep 14, 2023 at 8:54 AM mohd helmi <mohdhelmi.hasmuni@gmail.com> wrote:
Dear Expert,

I have difficulties regarding material inspection. Now client reject my material inspection due to thinner plate not same with DO? for examples plate purchase 10mm now coming around 9.75mm, which code can I am refer to? 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHjDVH_%2B3Q%3DbxS5_3jTNHsFR9Xc8PznxNkdUgZzbFbY3JBuF6g%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAG5OBYFSPi_WMa0BaZw6LYwXTVXB26BpTcjy%3Do_KP%2BGKPonU2Q%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...