[MW:34536] Alloy steel -Tube and Cladded tube sheet


Need guidance for PWHT - 

Code of Construction - ASME SEC VIII DIV 1 
Job - Heat exchanger 
Material - Tube -SA 213 T11 - 19.05 OD X 2.11 THK 
Tube sheet - SA 336 F11 CL2 , Cladded with Alloy 600 

Tube -Tube sheet joint configuration -  Groove and Fillet - 2mm -45Deg Vee with 2 mm fillet 

Welding Process proposed - GTAW  
Welding  filler metal  proposed- ERNiC3 
Query -
We reviewed the PWHT exemption in Table UCS-56-3  for P-No. 4 materials and UW-40 (f)(g) for Nominal thickness consideration and PWHT requirement 
Here nominal thickness is  Tube thickness (2.11mm )  as per UW-40 (f)(g)

Pl  advice for PWHT exemption for  above configuration of Tube to tube sheet PWHT  wrt Table UCS-56-3  or any other ref in ASME SEC VIII DIV 1 

Thanks 
Vishwas - IWE 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b7222382-b1ab-4e82-9c00-ad031880022en%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...