Re-do All NDT Performed before rolling. Volumetric NDT Results should compare with before rolling. (Ex. Radiographs before and after compare it)  

Thank you, 
Regards, 
S.SENTHILKUMAR


On Wednesday, 27 September, 2023 at 07:22:42 pm IST, RAJESH KUMAR <rajeshkumarbhaskara@gmail.com> wrote:


Dear Expert,

During a site observation, a subcontractor's carbon steel shell (EH36, thickness 40 mm) was found re-rolled due to ovality after 100% of the NDT(UT&MPI) long seam welds. Many stresses come and grain boundaries are stretched after rolling such a thick joint.Any experts please advise.

Standard - DNV-OSC -401
Construction specifications - AWS D1.1
image.png


Thanks & Regards

Rajesh

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMtcSfO5WESSOFt_GNicQH25ffSSuAHHGSSfNkCMp2FRCzLAMQ%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...