Tuesday, February 21, 2023

Re: [MW:34025] 6061 aluminum WPS PQR

Hi,
The attached files might be useful to you.

Thanks& Regards,

(Karthik)
Karthikeyan.S
M: +66-892512282


On Tuesday, February 21, 2023 at 10:11:40 AM GMT+7, kadir...@gmail.com <kadirgodil@gmail.com> wrote:


Dear group members,
Can someone share me a sample of wps pqr copy for my reference for the welding of 6061 for fillet and butt joint welding with process tig and mig.
thank you
sincerely,

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ff04a8dd-888e-4f5b-98c5-da432e0fa6d2n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...