1. you can bolted U or C clamp suit to fitup
2. or shop weld, flang can keep bottom na pipe freely fitup, to keep gap kept filler wire. and weld..

On Wednesday, February 1, 2023 at 5:43:55 AM UTC+3 kkmec...@gmail.com wrote:

Dear Experts,


Please find the attached pictures if there are alternate options for Fit up as tacking has been done directly on the Flange.


Please advise.


Best Regards,

 

Krishna Kamal Nayan  


 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c23736a-4423-42d1-8915-7ca26990424fn%40googlegroups.com.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...