Thursday, February 2, 2023

Re: [MW:33980] SFA 5.36 - FCAW consumable for Carbon steel

The electrodes will continue to be listed in SFA-5.18/SFA-5.18M, ASME SFA-5.20/SFA-5.20M, ASME SFA-5.28/SFA-5.28M, and ASME SFA-5.29/SFA-5.29M

On Thu, 2 Feb 2023 at 08:42, Zacharias Rohith Joseph <rohithjoseph18@gmail.com> wrote:
What does this mean by withdrawn from section 2C 

Where should we check the consumable properties now ? 




--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubn0c9QhavYmd%3DBPNxqGuCADaZ1h8%3D6CTMgR0hzkSt6PUQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...