Dear sir ,

I don't think you required different calibration block for CS/SS.

Because if you look at Hardness tester working principal that  A hardness test is performed by pressing a specifically dimensioned and loaded object (indenter)
( Which is independent of material either CS/SS)  into the surface of the material you are testing. The hardness is determined by measuring the depth of indenter penetration or by measuring the size of the impression left by an indenter.

If I am wrong .Please let me Know.

On Tuesday, February 7, 2023 at 8:28:31 AM UTC+5:30 furkan topaloğlu wrote:
Dear Experts,

I would like to ask a question regarding the hardness test on Stainless Steel and Carbon Steel.

Do I need a different calibration block for SS / CS or another probe for these different types of material?

Can I use the same probe on the SS and CS material without additional calibration ?

Could you please inform me with technical background ?

Thanks in advance. Regards

--

Regards / Saygılarımla

 

Furkan TOPALOĞLU

Metallurgy and Material & Welding Engineer

Phone : +7 916 524 21 02

              +90 539 437 88 03

E-Mail : topalogl...@gmail.com

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/3fb01dd4-b472-4152-a39d-0b0743ca1d7bn%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...