Re: [MW:32580] SA 516 GR 70- AVOIDANCE OF PWHT - 40 mm thickness

Normally the use of Nickel electrodes to avoid PWHT was practised in the SR(self reinforced) Nozzles where the vessel is not PWHTed and the Nozzle weld requires PWHT. Experts can throw some light on the C seam and any code restrictions.

Thanks & Regards

J.Gerald Jayakumar



On Friday, 29 October, 2021, 11:53:02 am GMT+4, Vishwas Keskar Welding Manager WELDING <vvkeskar123@gmail.com> wrote:


The vessel details are 
MOC - SA 516 GR 70 
DIAMETER- 4020mm
LENGTH - 37 MTR
MDMT = - 50 Deg C to  + 250 Deg C 
SERVICE - Non lethal /No Hydrogen Service 

We are proposing Vessel length build up as per FURNACE LENGTH CAPACITY(24 m maximum) and one joint WITHOUT PWHT  ( JOINING PWHTed sections earlier at site )
Proposal - 
1.MOC - SA 516 GR 70 
2.BUTTERING - ENiCrFe2 on 24 m section end and other at 13 m section end)
3,PWHT (section PWHT - One of 24  length and other 13 m)
 of  - 620 Deg C - 125 MINUTES 
4.Bevel preparation 
5.NDT - DPT 
Welding at site ( 24 m section with 13 m section) - ENiCrFe2 OR E309 
6.NDT - DPT AND UT

Expert opinion please  and share experience if any 

Vishwas 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdca7c90-9d2b-4df4-a685-5e7745a76351n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...