Re: [MW:32580] SA 516 GR 70- AVOIDANCE OF PWHT - 40 mm thickness

Thanks for Sir.
Pl help for ref for Code or Code case.

On Fri, 29 Oct 2021, 21:40 pgoswami, <pgoswami@rogers.com> wrote:
Sec VIII,Div1:-
40 mm thickness calls for PWHT irrespective of service,  lethal or Non- Lethal. 
Would like to see in  DIV1,which code clause or code case,  allows application of buttering on C.S, PWHT of individual sections, welding of the closing seam by austenitic filler metal with no PWHT.

Thanks. 
P.Goswami. 




Sent from my Bell Samsung device over Canada's largest network.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/617c1ce1.1c69fb81.e31de.34e7SMTPIN_ADDED_MISSING%40gmr-mx.google.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADder3N4t9gCO%2B_BeK9hm%2Bh8G-U1tcHrxSHzqOyrmLiOqwxLFA%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...