[MW:32577] SA 516 GR 70- AVOIDANCE OF PWHT - 40 mm thickness

The vessel details are 
MOC - SA 516 GR 70 
DIAMETER- 4020mm
LENGTH - 37 MTR
MDMT = - 50 Deg C to  + 250 Deg C 
SERVICE - Non lethal /No Hydrogen Service 

We are proposing Vessel length build up as per FURNACE LENGTH CAPACITY(24 m maximum) and one joint WITHOUT PWHT  ( JOINING PWHTed sections earlier at site )
Proposal - 
1.MOC - SA 516 GR 70 
2.BUTTERING - ENiCrFe2 on 24 m section end and other at 13 m section end)
3,PWHT (section PWHT - One of 24  length and other 13 m)
 of  - 620 Deg C - 125 MINUTES 
4.Bevel preparation 
5.NDT - DPT 
Welding at site ( 24 m section with 13 m section) - ENiCrFe2 OR E309 
6.NDT - DPT AND UT

Expert opinion please  and share experience if any 

Vishwas 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/bdca7c90-9d2b-4df4-a685-5e7745a76351n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...