Re: [MW:32493] interpass temperature

Client specification always takes precedence and is mandatory.

For structural Application according to AWS D 1.1 gives the same requirement.


Inline image

 Maximum interpass temperature according to AWS D1.1 as mentioned in it based on Hardness value;

Inline image

Please select based on the requirement.

Thanks & Regards

J.Gerald Jayakumar




On Monday, 23 August, 2021, 08:46:25 am IST, Rameez khan RK <rk.rameezkhan21@gmail.com> wrote:


Hello Experts,

Can any one tell me about interpass temperature for carbon steel pipe as [per code and standards.

WE facing one issue here our Approved PQR interpass temp. is 290 but in WPS its mention 340 c so please defined and what is actually interpass temp as per codes per standards.


thank you   

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0c475dd0-ecd8-497c-a281-d0094ac7fa61n%40googlegroups.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...