Re: [MW:32489] Welder Qualification

API 1104 does allow for welder qualification of butt weld joint only by RT (API 6.6.1) it also allows welders to be qualified under ASME SEC. IX, which allows RT. 
BUT, it depends on what they are being qualified to weld on. If they will be welding on natural gas facilities, they will be required to have been qualified by destructive testing. (Per CFR requirements).

Thanks,

Chip Frizzell 

Price is what you pay-value is what you get. 
Seldom does the lowest price result in the best value!

Sent from my iPhone

On Aug 25, 2021, at 1:46 AM, qaqcbarmer mech <qaqcbarmer@gmail.com> wrote:


Is it mandatory mechanical test qualification for welders as per API 1104

Qualification by RT is acceptable ?.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d63d71b8-0ea7-412b-aa06-f4d2b4508b2fn%40googlegroups.com.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...