Re: [MW:32486] Multi process PQR to Single Process WPS

Ref 5.2.2 may be useful

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  CSWIP 3.1,
ISO 9712 Level 2 in VT,
ASNT-Level II in PT,MT,RT & UT,
LA ISO 9001-2015,
International Welding Engineer. 
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349


On Tue, Aug 24, 2021 at 9:55 AM Manikandan J <mechmani22@gmail.com> wrote:
Hello Experts,

I have existing PQR having combination of GTAW+FCAW process as per AWS D1.1-2015 Edn.

Can I write the WPS by using only FCAW process?

There is no clause in AWS D1.1?

Expecting your response with clause reference.

Regards,
Manikandan.
India.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPdGVmNzcM-x3rPHBA-oxx%2B%3Dyz%3DH0EKA0kjO691UW1Zx3VvhTA%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eMBeAwxEz70_vdvgYP%2B5fVV_jUwsvSwVjHAWOVMXRnVZQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...