Wednesday, May 26, 2021

Re: [MW:32391] welding guide for 4145H API-7

DEAR Sir, 

It is D&H Secheron make CNM Spl M product suitable for this welding. 


Thanks & Regards, 





On Fri, May 21, 2021 at 8:22 AM Mohd Siraj <mohd52100@gmail.com> wrote:
gents,

pl advise welding of 4145H, thk-25mm dia-8"

Electrode selection,Preheat,PWHT...

with SMAW, or SMAW+GTAW

Mohd.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d53a0cd0-dfec-4bd9-a533-1a53ace0ac86n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOVB-ER0aAmmp4G0NXkiEjDgYRtaXt01iVgso4kjwcf66ZoBVQ%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...