Re: [MW:32372] ASME BPV Sec V // T-224 SYSTEM OF IDENTIFICATION ON RT FILMS

Adding to Raghuram's comments - Any fogging or flasher shall not be used as ID on Radiographs in ASME Jobs. 

Thank you, 

Regards, 
S.SENTHILKUMAR


On Friday, 14 May, 2021, 11:02:44 am IST, Raghuram Bathula <raghurambathula@gmail.com> wrote:


This essentially be a permanent identification on each radiograph, no markings or stickers will be allowed for mandatory identification traceable to the film


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CADxVubmSvFBi%2B%3DrWbhZFnqf6RmTX0Qp3xdAfhL_NpdN_YPM%3Dug%40mail.gmail.com.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...