Dear Experts,

     At the site 308L filler wire used for the Pipe joint between 304L and 316L.  After doing the PMI QC rejected the joints and suggesting to use 316 filler.

   Experts kindly share the details of the code reference to accept or any procedure to avoid cutting 20joints.

--