Monday, February 18, 2019

Re: [MW:29119] Re: Equivalent ASTM material for EN S275JR

As per AWS D1.1 unlisted material subjected to New WPS  i agree.
but if 275JR to 275JR wps can we  considered to other grades those material impact properties  are not effecting (temp  )
 Can we consider   these are  single Group (235JR,,275JR,355JR) and weld wrto 275JR approved WPS.


On Thursday, May 7, 2015 at 9:39:17 AM UTC+4, aru ara wrote:
Dear,

you cannot get exact equivalent.

But nearby grade is ASTM A36   

ELAVARASAN ARUMUGAM
Mechanical Engineer 
 

On Wed, May 6, 2015 at 9:45 AM, R R Menon <ranjith....@gmail.com> wrote:
Hiii

its equivalent to ASTM A529

On Saturday, 23 July 2011 15:16:35 UTC+3, PRAMODH NAIR wrote:
Experts,
 
Could you please give me the equivalent ASTM material for EN S275JR with reference code document.
 
Regards
Pramodh

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-weld...@googlegroups.com.
To post to this group, send email to material...@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/394a3b77-8a49-4504-8a9f-4c150b4ba3d8%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...