[MW:29109] were to use longitudional bend test and transverse bend test

in asme sec 9 transverse and longitudional bend test are given in code it is mention when there is marked difference bw bend property of two base metal or weld metal than in lieu of transverse.
sorry i didnt unserstand this clause

--