As stated by fellow members, the obvious reason seems to be low productivity with associated higher cost of shielding gas (Pure argon). Although there is no restriction by the code or standards such as AWS D1.1, D1.3 or EN 1090. 
E.g. there is possibility to have a thin tubular connection with 1-2 mm but joint according to AWS D1.3 where you have no other choice.
although with bulk of welding joints, hundreds of weld runs require a high weld deposition which is not possible by TIG even it get automated

TIG is beneficial to have lower heat input which is merely a prime consideration for most of structural steels according to AWS D1.1 or other codes/ standards.
Unfortunately, most of people understanding on structural welds is welds with least precautions or lets say they are easy welds. However, in other scenario they are having more critical requirements according to AWS code compare to ASME Section IX in terms of essential variables.
 
Thanks & regards
Sandeep Kumar

On Tuesday, February 19, 2019 at 1:48:40 PM UTC+3, dinesh AWS-CWI ,CSWIP 3.1,NDT II wrote:
Dear sir,

Looking for advice why TIG welding not using for structural welding generally.

Please advice ahead.

Thanks & Regards

DINESH VITTHAL SOMWANSHI

BACHELOR IN MECHANICAL ENGINEER


Skype = dinesh somwanshi

असो द्यावी दया तुमच्या लागतसे पाया.

*Pray for others, sometime, You might never need to pray for yourself
again.....*

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...