[MW:29151] SSRT (Slow-Strain-Reducing-Tensile) Testing in lieu of HIC/SSC

Dear All,
Recently through technical articles i came to know that some of the Oil & Gas industries are using SSRT (2 days) in lieu of HIC test (7 days) and SSC test (30 days) due to time consuming and some times HIC/SSC are not a full proof method of ascertaining that even after sample passes in HIC/SSC test, it will not fail in field. 

Is it true that through SSRT we can avoid HIC/SSC testing for sour services. What is the acceptance standard for this SSRT test?

Requesting to guide on this subject.

Regards,
Devang Majithia

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...