Ok, please see:
Preheat: NONMANDATORY APPENDIX R. Of Section VIII Div. 1
PWHT: UW-40; UCS-66; Table UCS-56-1 of Section VIII Div. 1
Interpass Heating: QW-406 of Section IX.
Regards!.

El 30/06/2016 03:16, "williamswilsonp" <williamswilsonp@gmail.com> escribió:
Dear experts

Please reply with your suggestions for the below mentioned query,

We are going to conduct the pqr qualification test for base metal - SA 516 gr.70(P 1 Gr.1,2 to P1 Gr.1,2) as per ASME Sec.IX

Thickness of Base metal is 20 mm

Which type of heat treatment is required during welding
Preheat
Interpass heating
PWHT

Thanks in advance







Sent from Samsung Mobile

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1ct7lngbp86f3jeh5k3iiaxw.1467270419942%40email.android.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAO5ZurLxwWddOyN9upx3m2whHXhzSYiDTUyYGiXgXbgYE8kfEg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35742] PQR- Chemical testing requirements

Good Day to all, Reference std: ASME SEX IX Material ASTM A106 Gr B Pipe Dia and thickness: 2" and 8.74 mm. Service Fluid: Normal fluid...