lower limit shall be derived from ASTM A370 with comparison of minimum
tensile strength.
On Sun, Jul 3, 2016 at 8:57 PM, Ankit Gandhi <asgandhi.90@gmail.com> wrote:
> Dear sir,
>
> As per Hardness procedure we are often seeing that for P1 material 200 BHN
> P4 material 220 or 230 upper limit, but in no case we i have seen lower
> limit for hardness.
>
> Normally after PWHT Forging material hardness is going down distinctly may
> be 130-140 BHN.
> So Please let us know what is lower limit for hardness and what is reference
> document for that?
>
> Regards.
> Ankit Gandhi.
>
> --
> http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
> The views expressed/exchnaged in this group are members personel views and
> meant for educational purposes only, Users must take their own decisions
> w.r.t. applicable code/standard/contract documents.
> ---
> You received this message because you are subscribed to the Google Groups
> "Materials & Welding" group.
> To unsubscribe from this group and stop receiving emails from it, send an
> email to materials-welding+unsubscribe@googlegroups.com.
> To post to this group, send email to materials-welding@googlegroups.com.
> To view this discussion on the web visit
> https://groups.google.com/d/msgid/materials-welding/d9c7d4b9-9e5d-49a9-8aee-6caee5dd0657%40googlegroups.com.
> For more options, visit https://groups.google.com/d/optout.
--
Thanks, & With Best Regards,
Dharmesh MISTRY
+91 9820735814
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMPvC1AOynzLqgEunYdCK281iU6jx-Bw6eRdhQ9kBzgzFpnztw%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment