PWHT is not essential for Welder and He need not bother about PWHT. Confusion will come in recording variable and preplanning is very much essential for each joint
--Yes you can.
Section IX does not dictate the form of the WPS (or the PQR for that matter) but only dictates the variables or components that must be addressed. A single WPS can be written for both conditions as long as the essential variables and non-essential variables are addressed for both conditions (and if appropriate, supplementary essential variables). I have frequently seen WPS's of this type and upon review have approved them on the basis of addressing all required variables. In a previous job, it was not uncommon to weld a single coupon, split it into two parts and test one half with PWHT and the other tested as welded and then write a single WPS. However, a single welded coupon is not required.
The biggest problem is to avoid confusion for the welder caused by a too complex a WPS. Remember that the ultimate purpose of the WPS is to provide guidance to the welder on how to complete the weld.
Don't import your personal bias into requirements for qualification. Apply what is required by the Code and, if necessary, the ever annoying customer.
Enjoy.
From: 'Dinesh Gaur' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: Monday, July 18, 2016 10:46 PM
To: materials-welding@googlegroups.com
Subject: Re: [MW:25116] ASME Section 9
Dear Mr.Parvan
Can you brief that on what basis you can made a single WPS?
As per ASME Sec IX, You Can"t.
On Tuesday, 19 July 2016 6:41 AM, "p_chavdarov@mail.bg" <p_chavdarov@mail.bg> wrote:
Yes, you can, as long as all other variables are equal.
Best regards
Dr. Parvan Chavdarov
----- Цитат от Kannayeram Gnanapandithan (kgpandithan@gmail.com), на 15.07.2016 в 06:13 -----
Having 2 PQRs ,one with PWHT and another without PWHT. With these 2 PQRS, can a single WPS be made addressing both conditions by keeping other variable in the order..
THANKS & BEST REGARDS,
KG.PANDITHAN, IWE, AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eO%3DEaB2TgXQB8Usw52QYPOdFDvP_9ZrGPkUJNLKSdL%3DLQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
-------------------------------------
Mail.BG: Безплатен e-mail адрес. Най-добрите характеристики на българския пазар - 30 GB пощенска кутия, 1 GB прикрепен файл, безплатен POP3, мобилна версия и други.--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/30bb268b1e74c1e08ca07b408bda2bc3.mailbg%40mail.bg.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1017866144.1112415.1468899987374.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BY2PR0301MB154162DAF1A4EB903EF3EFC3A1370%40BY2PR0301MB1541.namprd03.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAJzm4eOU61mcWbY0BVnkkozvvPKfY_P23RmMz0kMNvAtUAE7bA%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments