1) You can't use API1104 WPS for ASME sec IX welder qualification.
2) In API 1104 and ASME sec IX there are many difference essential variables for single qualification/ Multiple Qualification/ Mechanised welder with filler addition & Automatic welding without filler metal addition
(e.g: OD grouping, Thickness groping, Filler metal grouping, Joint design not meeting the requirement of ASME sec IX)
You can proceed the welder performance according to respective code approved WPS.
Regards,
Pravin Nimbalkar
Welding Engineer
BILFAL heavy industries ltd. KSA
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/efee9d9c-dd9b-4ebc-94e7-8f382bcf146e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment