ASME VIII says tack welders shall be qualified.
Sec. IX not specifically mentioned.
So both in refinery & power plant , as per ASME IX , QW-461.9 we followed 5F position (pipe to plate 45 degree inclined) to qualify tack welders.
Best Regards,
JIJILAL K.M.
QA/QC Manager,
Thai Jurong Engineering Ltd,
KCE SPP Project,Thailand
#096 786 0129
On 29 July 2016 at 21:10, César Alexis Viteri Pérez <alexis_viteri@hotmail.com> wrote:
Be sure that tack welders dont open arc out if bevel.
Date: Thu, 28 Jul 2016 21:05:20 +0300
Subject: Re: [MW:25156] Re: Tack welder qualification
From: dilintas@gmail.com
To: materials-welding@googlegroups.com
...if they remain in place...Sent from my BlackBerry 10 smartphone.
From: anthony chundalSent: Πέμπτη, 28 Ιουλίου 2016 - 13:04To: Materials & WeldingReply To: materials-welding@googlegroups.comSubject: [MW:25155] Re: Tack welder qualificationDear Sam,As per ASME Sec VIII-Div-1, UW-31(c), tack welders need to be qualified.Regards,Anthony.
On Tuesday, December 13, 2011 at 8:48:37 PM UTC+4, samshuddin k wrote:Dear Experts
There is any clause in ASME Sec. IX for tack welder qualification.
Which Code explains tack welder qualification for piping
regards
Samshuddin.K
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/cc0d08ba-e64a-49a5-9402-5354a48c9a48%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/20160728180520.6713423.18949.3894%40gmail.com.
For more options, visit https://groups.google.com/d/optout.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BLU183-W15A51C161BD8FC45EFA3828F010%40phx.gbl.--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHggn7m8YPraKd08aZ-M3aeuLvV5EwVn0LVmLBnhzE0p5w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Comments