Re: [MW:20684] Incoloy 800 stub to tube welding

Please clear the following:

  1. Is it a new construction or a maintenance (repair) job...?
  2. What are your welding parameters...?
  3. By root cracks do you mean cracks are in the weld metal or fusion boundary cracks...?

Best Regards

Ramin Kondori

Sr. QA/QC engineer

Yadavaran Oilfield Project

SIPC (SINOPEC)



On Sat, Apr 26, 2014 at 11:40 AM, Raghuram Bathula <raghurambathula@gmail.com> wrote:
what is the filler?, can you share joint sketch?


On 26 April 2014 12:17, 'V G Pathak' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Hello all welding experts,

We are welding fillet of incoloy 800 stub to tube with tube OD 12.86 mm and thickness 2 mm with GTAW and 99.999% purity argon gas with correct filler wire. When we do micro exam, we find root crack and LF.

We have been unable to resolve this issue for past 3 months.

Can any one give suggestion on how to overcome this problem?

Your earliest reply shall be highly valuable.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...