[MW:20703] RE: 20701] Re: Thickness Range Qualified by Welder - ASME Sec. IX

As of the 99 Addenda there is no minimum qualified thickness for weldor qualification.  The minimum thickness will be that of the applicable PQR. 

 

Remember diameter rules of QW-452.3 still apply.

 

John A. Henning

Welding & Materials

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jhonn Zambrano
Sent: Tuesday, April 29, 2014 11:08 AM
To: materials-welding@googlegroups.com
Cc: vjadhav@ccc.ae
Subject: [MW:20701] Re: Thickness Range Qualified by Welder - ASME Sec. IX

 

Hi everybody, somebody knows if there is a minimun in the thickness of weld metal qualified, because in the Table QW 452,1 b, there's only a maximun but not a minimun.

 

 

Thanks

 

 

Jhonny Zambrano

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


______________________________________________________________________
The information in this email is confidential, and is intended solely for the addressee(s). If you are not the intended recipient of this email please let us know by reply and then delete it from your system; you should not copy this message or disclose its contents to anyone. The internet can not guarantee the integrity of this message. HAMON (and its subsidiaries) shall (will) not therefore be liable for the message if modified.
______________________________________________________________________

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...