MR.K.KANIKUMAR,
you can use as below,
Beam, material S275JR (or) EN10025 ----> E6010 or E7018
Rack, Material- E335 (or) EN10025 -----> E 7018
i used this.
On Mon, Mar 24, 2014 at 10:08 PM, Kanikumar Kumar <kanikumar1989@gmail.com> wrote:
--Dear sir,Please refer the below materials, I have to weld with SMAW process.Can you please give us a proper electrode & if any special procedures have to be followed.
Kindly suggest me, which electrode i have to use?
Beam, material S275JR (or) EN10025.
,Rack, Material- E335 (or) EN10025.
Regards,K.KANIKUMAR.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
ELAVARASAN ARUMUGAM
Mechanical Engineer (ASNT Level II)
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Comments