Is a WPS is required for conducting WQT  :ANS : YES, WPS is req during the WQT
can we use a preliminary WQT  : ANS : NO
The WPSs shall be identical for all the essential variables, except for the
preheat temperature and PWHT requirements. or has an SWPS
adopted in accordance with Article V,ASME SEC-IX


On Sunday, March 16, 2014 10:23:06 AM UTC+5:30, mahammed javeed wrote:
Gentle men,

My question is regarding to the welders qualification test, My client is insisting to use a qualified WPS for qualification of WQT, Is a WPS is required for conducting WQT? or can we use a preliminary WQT or just follow the essential varialbles list as per ASME Sec IX?

Regards
M. Javeed
Quality supervisor

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...