Thursday, March 20, 2014

[MW:20388] RE: 20373] Welding of 3.5% Ni Steels

Mohit,
 
3.5%Ni (SA 203 Gr D& E) has excellent weldability and are proven materials for design/service temperature up to -101 DegC(-150 Deg F).These steels are perfectly weldable with heat input control(Q-2-2.5 Kj/mm, Max) and with matching welding consumables. See the attached datasheet for general reference.
 
Also see the earlier  discussion on this material in this forum.
 
It would  be good to know what're the applicable design requirements for 3.5% Nickel steels.
 
Thanks.
 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Specialist
Ontario, Canada
pradip_goswami@yahoo.ca
 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Mohit Aggarwal
Sent: Wednesday, March 19, 2014 1:35 AM
To: materials-welding
Subject: [MW:20373] Welding of 3.5% Ni Steels

Dear Experts,      
Please let me know From where I found literature for weldability Of these steels & related issues...

Regards
Mohit Aggarwal

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...