Saturday, January 31, 2009

[MW:1487] FW: 1485] HYDRO TEST OF VESSELS

Rushabh,

I forgot to reply your below concern,

Change in vessel length doesn't affect the HOLD time.

Regards
Somesh
-----Original Message-----
From: Somesh Kumar Pandey
Sent: January 31, 2009 3:53 PM
To: 'materials-welding@googlegroups.com'
Subject: RE: 1485] HYDRO TEST OF VESSELS

Rushabh,

UG-99 of VIII-1 does not specify a minimum hold time for hydrostatic
test pressure. It all depends on the time needed to fully inspect the
vessel to ensure no leaks are present.
You have to also check the client specifications; they often specify
minimum hydrotest duration. For vessels I recommend 1 hour stabilization
at maximum pressure.

Regards

Somesh
-----Original Message-----
From: materials-welding@googlegroups.com
[mailto:materials-welding@googlegroups.com] On Behalf Of Nick
Sent: January 31, 2009 3:17 PM
To: Materials & Welding
Subject: [MW:1485] HYDRO TEST OF VESSELS


Does ASME define the HOLD time required for holding pressure during
HYDROTESTING of vessels?

If yes does change in vessel length affect the HOLD time?


Regards
Rushabh C. Kapadia


This e-mail, including any attached files, may contain confidential and privileged information for the sole use of the intended recipient. Any review, use, distribution, or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive information for the intended recipient), please contact the sender by reply e-mail and delete all copies of this message.

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...