Dear Nilesh,
 
 
             You go through the following link. I hope you will get a good idea.
 
 
Regards
Prabhakar. S

 
On 1/12/09, Darji Nilesh (Mumbai - Machinery) <N.Darji@ticb.com> wrote:

 

Dear Friends,

 

Requesting you help to furnish Eq. ASTM Grades for the following material: -

 

  1. 1.8963 (Is it better than SA 242 Gr.2 ??)
  2. 1.7218 (Required material by Process data sheet is A 1045. Material 1.7218 is better than A 1045 ??)
  3. 1.0037 (Required material by Process data sheet is CS-Epoxy painted. Selected material by Vendor is 1.0037, Is it better option ??).

 

Matter is little bit urgent so, kindly furnish your response before noon.

 

With regards,

 

Nilesh.

 

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...