[MW:1479] CHLORINE INSTITUTE PAMPHLET 6 CLASS II - Requirement

Dear All,

I have one piping class in LTCS material which is to be used for CHLORINE GAS service.
With Design condition as follows:
Min 1.84 MPag@ -39 degC
Max 1.38 MPag@ 200 degC
Rating : 150#

For this class our Licensor along with code ASME B31.3 has given requirement of CHLORINE INSTITUTE PAMPHLET 6 CLASS II.
Dear members can you explain me what exactly is this requirement, and if its applicable only for valves or also for other fittings.
Thank You & Kind Regards
Vijay Kadam

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...