All info is available at api website


From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of G Padmanabhan
Sent: January 27, 2009 10:06 AM
To: materials-welding@googlegroups.com
Subject: [MW:1474] Re: Required API 650 personal for Bahrain

Dear Shriram,
Where we can take API Training course in  India.

On Tue, Jan 27, 2009 at 7:37 AM, SHRIRAM PURANIK <stpuranik@gmail.com> wrote:
There is as such no API 650 qualification. Its API 653. You can search list of qualified persons on www.api.org
 
Regards,
 
Shriram T Puranik
API 510, 570, 571, 577, 580, 653
 


 
On Mon, Jan 26, 2009 at 6:06 PM, Rajesh Shetty <shettyrajeshbabu@gmail.com> wrote:
Dear Friends,
 
Anybody knows person having API 650 qualifications ready to give service a company in Bahrain, for a short period?
 
Please send details if you know somebody
 
With Best Regards
Rajesh
00973 30934717

On Sat, Jan 24, 2009 at 3:58 PM, Ravi Ronanki <ravi.ronanki@gmail.com> wrote:
Dear Friends,
 
 
Kindly let me know from which website or blogspot the fabrication tolerances for Pressure Parts and Structural Items can  free downloads be available.
 
The matter is urgent.
 
 
Regards,
 
 
R.Ravi

 
On 1/22/09, Charles Nelson II <charles.nelson.ii@gmail.com> wrote:
Hello Muhammed,
 
In response to your question below, X-ray radiography is you best choice due to quality issues. 
 
The second question is slightly difficult to answer as each tube/generator has different characteristics, as also the film and geometric variables have.  In referencing one of my resources, a higher end X-ray tube rated at 400-450 kV could theoretically penetrate thickness up to roughly 300 mm.  The lower limit for 50 kV is approximately 20 mm.
 
I usually work with castings from 30 mm to approximately 75 mm, although, I primarily use digital radiography using a CMOS detector. 
 
A generally accepted method of ensuring acceptability of a method is to demonstrate required sensitivity (i.e. hole-type or wire-type image quality indicators) per referencing code. 
 
I have a colleague that is better accquainted with thinner materials.  I will forward him your question and I will email you if I can clarify practical limits.

Thank you,

Charles Nelson


On Wed, Jan 21, 2009 at 10:50 PM, Muhammed Ibrahim <ibratech@gmail.com> wrote:

Hi friends,
 
Good morning,
 
I have a query regarding the radiography of aluminium.
 
X-ray or gamma ray is better for aluminium?
 
If x ray is better , what is the thickness range it can be done?
 
If gamma ray is better , what is the thickness range it can be done?
 
If anybody having the procedure, please forward

Thanks & Regards
Muhammed Ibrahim PK
 







--
Cheers

Rajesh B. Shetty
Bahrain




--
With Warm regards,

G.Padmanabhan
00967771103169

This e-mail and any attachments may contain confidential and
privileged information. If you are not the intended recipient,
please notify the sender immediately by return e-mail, delete
this e-mail and destroy any copies.

Any dissemination or use of this information by a person other
than the intended recipient is unauthorized and may be illegal.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...