[MW:1406] Re: Equivalent PWHT

Alternatively you may pwht carbon steel side vessel first to the requirements and then weld SS to CS using Inconel electrodes by qualifying the WPS.

Best Regards,
Francis Lobo
----- Original Message -----
From: sanjay <sanju2705@yahoo.com>
To: Materials & Welding <materials-welding@googlegroups.com>
Sent: Sun, 14 Dec 2008 15:55:50 +0530 (IST)
Subject: [MW:1398] Equivalent PWHT


Hi Friends,

I have a dissimilar material joint of P1 to P8, having PWHT. Thickness
of the joint is 75mm. As per UCS 56, we can perform PWHT at 620 Deg C
for 135minutes, but that will sensitise P8 material. So we want to
perform PWHT at 435 Deg C.

Please advice the duration of PWHT and how to arrive at that
duration.

Regards.

Sanjay Jain

--

"KLUB MJ Hunt, Search for India's First Movie Jockey"
For more details log on to http://www.zeecinema.com

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...