On 14 Dec, 15:25, sanjay <sanju2...@yahoo.com> wrote:
> Hi Friends,
>
> I have a dissimilar material joint of P1 to P8, having PWHT. Thickness
> of the joint is 75mm. As per UCS 56, we can perform PWHT at 620 Deg C
> for 135minutes, but that will sensitise P8 material. So we want to
> perform PWHT at 435 Deg C.
>
> Please advice the duration of PWHT and how to arrive at that
> duration.
>
> Regards.
>
> Sanjay Jain
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Sunday, December 14, 2008
[MW:1399] Re: Equivalent PWHT
Pl. check Table UCS-56.1 for alternative PWHT requirements!
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment