MDMT -46 °C

MOC: SA333 Gr6, SA 350 LF2, cl1, both are exempted from CVN impact as per UCS 66(g)

Consumables used are ER80SNi-1, and E7018 G as per SFA5.5 (both are tested at -60 °C with satisfactory values as per mfr data sheet)

However PQR impact testing required unless consumable are classified by impact tests at least at -46 °C by the applicable SFA as per UCS 67 (a) (2).

In this case E 7018-G (ETC PH 76S of Oerlikon) as per SFA 5.5 does not satisfy this rule.

In my opinion CVN impacts are required on PQR. Members please share your opinion/interpretation.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...