I have a dissimilar material joint of P1 to P8, having PWHT. Thickness
of the joint is 75mm. As per UCS 56, we can perform PWHT at 620 Deg C
for 135minutes, but that will sensitise P8 material. So we want to
perform PWHT at 435 Deg C.
Please advice the duration of PWHT and how to arrive at that
duration.
Regards.
Sanjay Jain
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---