Hi
Normally the filller metal will be the same for both. If any different filler metal has to be used, select the one which has the required impact properties at the MDMT you are looking for.
Thanks and Regards,
K.Rajagopal

 
On 12/3/08, SHRIRAM PURANIK <stpuranik@gmail.com> wrote:
Thanks, if impact is required then which filler metal to be used for qualifying WPS with different group and with same P no.
 
Regards,
 
S T Puranik

On Wed, Dec 3, 2008 at 12:01 PM, Muhammed Ibrahim <ibratech@gmail.com> wrote:
Group number is to be considered when impact is required.
 


 
2008/12/3 SHRIRAM PURANIK <stpuranik@gmail.com>

Can any body clarify for SA 240 TP 310S (P8 Gr. 2) + SA 240 TP321 (P8 Gr.1)  WPS to be separately qualified if I have separate qualified WPS and what filler wire to be used.
 
Regards,
 
S T Puranik

--
Shriram Puranik
 





--
Thanks & Regards
Muhammed Ibrahim PK
  --~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35748] Re: PQR- Chemical testing requirements

As answered by everyone, chemical is not required. Notwithstanding, please note that A-No. which denotes weld metal chemical composition is ...