Tuesday, May 27, 2008

[MW:798] Re: Dissimilar Group number/Thickness combination PQR as per QW403.5/QW403.6

Min qualified thickness can't be 1.5mm, when impact testing required.
Qualified thk range for P1G1 will be 6-12mm and P1G2 would be 12-24mm,
please refer the question again.

Dissimilar thickness combinations are quite common to qualify (in
particular for SR nozzle welds on equipment) per QW202.4

-----Original Message-----
From: Quality [mailto:quality@gpsoman.com]
Sent: Tuesday, May 27, 2008 10:28 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:797] Re: Dissimilar Group number/Thickness combination
PQR as per QW403.5/QW403.6


The qualified thickness range is 1.5mm to 12mm (2T) for P1G1to them
selves,
P1G2 to themselves & P1G1 to P1G2 combinations.

The maximum qualified weld deposit is 2t (to is deposited weld thickness

during the qualification).

If you qualify a procedure with different parent material thickness
(groove
weld), the thickness T can be considered based upon the tensile specimen

thickness (T) used for the destructive testing of the groove weld PQR.
In
short, qualification of different thickness of relatively less use in
ASME
Sec IX.

Normally none of the construction/ fabrication codes does not allow
difference in thickness more than 1.5T (of the thinnest). Any Thickness
welded above 1.5 will not be accounted in design.

Regards,
Sanjeevan
GPS


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...