[MW:765] Re: Joint Factor

 
Actually term is Joint Efficiency
For Full Radiography(100%)-Joint Efficiency is 1%
For spot radiography(85%)-Joint Efficiency is 0.85%

Regards
Sachin

On Thu, 08 May 2008 Zameer Mohammed wrote :
>Dear Friends,
>
>
>
>Whats is Joint Factor in Welded Pipes. We are procuring 24'', 36'' and 42''
>Welded Pipes (EFW). Our client is asking what is the Joint Factor.
>
>
>
>Thank you,
>
>
>
>Regards,
>
>
>
>
>
>Sabir
>
>>

Sachin.Sankhe
Engineer-Inspection
Aker Kvaerner-Malaysia
Mobile:012-2896901
Email1:Sachin.Sankhe@akerkvaerner.com
Email2:Sachin.sankhe@rediffmail.com


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35668] Selection of Filler/Electrode.

Dear Gentlemen, Kindly advise me as we have tube to tubesheet joint. Tube moc is incoloy 800 And tubesheet moc is F53 SDSS (Super duplex sta...

JS RED

Pages

Contributors

Blog Archive