Felt to caution people who prescribe the bolt coating.
In an inhouse test of Polymer coated bolt of of a reputed Japanese vendor, which was to perform 4000 hours of salt spray test as per B 117, did not meet the requirement though the vendor's test certificates prooved so. The inhouse test was performed as in one of the plant it was used and has peeled off while normal wrenching and never stood even 1/4 of the life period gauranteed by the supplier. Literally all bolting of the plant had to be replaced by the client.
The final recommendation is that it is ideal to have a phosphating coat and a galvanizing or zinc coat and the final coat to be fluorocarbon polymer coat which really stood well in acc. with B117 in the inhouse test and has been proven in few operational plants.
So as a caution note, it would be a good practice to go for multiple coat rather than single coat for the general call for such coating requirements.
I do not want to name the companies explicity in this list for obvious reason.
Readers' experienced views are welcome.
With regards,
Kannan.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment