[MW:637] Re: Etch structure acceptance in IGC test per ASTM A262

It has something to do with the applicability of the test. Practce C vs. E

Practice C is applied for wrought, Cast or weld metal structure while, E is
applied for wrought or weld metal. thus, the difference remains in
acceptance criteria.

Best regards,

Prasad Joshi
e-mail: pjoshi@technip.com
Phone: +971-(0)2-611-6643



Raghuram Bathula
<raghurambathula@
gmail.com> To
Sent by: "Materials & Welding"
materials-welding <materials-welding@googlegroups.com
@googlegroups.com >
cc

29/02/08 07:24 PM Subject
[MW:636] Re: Etch structure
acceptance in IGC test per ASTM
Please respond to A262
materials-welding
@googlegroups.com



yes but ditch and Interdendritic ditch both are different and it
didn't state anything about Interdendritic ditch structure

Save a tree...please don't print this e-mail unless you really need to.

Save a tree...please don't print this e-mail unless you really need to.


--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
-~----------~----~----~----~------~----~------~--~---

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...