Hardness testing based on rebound velocity principle is very common in process industries to check the surface hardness. However,if you need to check the section hardness Ultrasonic based HT is a good option.
 
regards,
gopalsankar

tamma reddy <tsr_52@yahoo.co.in> wrote:
Dear Venu,
 
Thanks for your reply.
Just I would like to know, whether this rebound principle is recognised in construction industry and being used else where or not.
 
I have studied in depth about this hardness tester and there are other models like UCS working on the principles of ultrasonics and third one is TIV. However, this rebound principle is well known to mechanical industry. Also, ASTM standard is available on digital hardness tester working with rebound principle.
 
Here, our dept is not allowing this type of hardness tester for hardness check at SEZ refinery construction. However, I am trying to convince HOD and other colleagues to introduce this tester. 
 
Any way, pl. note my personal mail id also and send mails. Convey our best wishes to all your family members.   
 
Regards,


T S Reddy
Mobile: 919998215568
India


----- Original Message ----
From: juttada venugopal <jamsvenu@gmail.com>
To: materials-welding@googlegroups.com
Sent: Sunday, 2 March, 2008 5:10:47 PM
Subject: [MW:644] Re: Hardness by Equotip

Dear Reddy,
 
Equotip is digital based, unlike Poldy which is mechanical based.
(1) This needs the surface to be smooth, so that rebound shall be proper for its analysis.
(2) The rebound ball is few grams so thickness of the part shall not be an essential criterion. There is facility for angle setting in this instrument, 0deg  i.e., is hitting the targets vertically down, and other angle hitting facility exists
 (3) Equotip is supplied with thick round calibration block, valves on it are mentioned to match with for calibration purpose.
 (4) These are commonly used in maintenance sections of the plants. It only gives the valves of the hardness, so hope no implications of restriction of any codes prevails.  
 
Hope I have answered your questions.
 
Regards,
 
Venu
Singapore
================================================================
On Sun, Mar 2, 2008 at 5:26 PM, tamma reddy <tsr_52@yahoo.co.in> wrote:
Dear Friends,
 
Can any one through light on the following queries of digital hardness tester (Eqotip/TIME Group TH 160, HLN-11A/Krautkramer etc.)
 
1. Can weld joint hardness check up with rebound test principle
2. what is the minimum thickness of test specimen required for hardness check with above equipment (working on Rebound principle)
3. What are the calibration requirement of above instruments
4. Are they supported by any project construction codes/ standards
 
Regards,

T S Reddy
Jamnagar


Chat on a cool, new interface. No download required. Click here.

Now you can chat without downloading messenger. Click here to know how.

Never miss a thing. Make Yahoo your homepage.
--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...

Re: [MW:10788] ON PLOT PIPING & OFF PLOT PIPING

Piping systems involved for the flow lines and gathering lines from the well head isolation valve to the production facility or processing plant isolation valve are determined as OFF PLOT. ON PLOT defines piping system in the processing plant and production platform. ANSI/ASME B31.4 applies for off plot piping system. B31.4 allows the use of either API 1104 or ASME section IX (as appropriate). However, occasionally, a very small system such as piping within 500 feet of a processing plant (some client also said 400 feet) may be declared B31.3 rather than B31.4. When B31.3 is invoked, only ASME Section IX is used. before you decide which code to use for welding procedure and/or welder qualification for pipe welding, you have to know the design and construction code applicable to the system. Please read far enough into scope and diagram illustrating the application of either B31.3 and B31.4 hope this helps rgds 2011/4/21 pradip kumar sil < pradipsil@gmail.com > Dear all, ...