  Dear mustak  patel
I think by CE u mean Carbon Equivalent. As per ASME Sec IX there is nothing specified for CE tolerance in WPS or WPQ.
CE is required to find out the preheating temp. of the job...
in British or japanese standards its given + 0.003 % Max ?? surprising. what is the british standard - EN 288 ?
How can CE be such low - 0.003. For CS, the CE is 0.2 -0.4

Regards

Prem Nautiyal



On Wed, 19 Mar 2008 mustak  patel wrote :
>
>Hi guys
>
>What is the tolerance given in the AMERICAN CODES for CE value for applicability of WPS and welder qualifications? Is it an essential variable? I think in British or japanese standards its given + 0.003 % Max.
>
>Appreceiate any feed back.
>
>Thanks and Regards
>
>
>On Tue, 18 Mar 2008 rajesh patel wrote :
> >
> >dear Friebds,
> >
> >I am a silent but regular reader of the mails shared
> >by group memebers. I am greatful to receive such
> >valuable information from the various people from
> >every corners of the world. Through this group,I even
> >recd some mails from my old couligues with whom i lost
> >all contacts since last so many years.
> >
> >I may not be replying or sharing anything but i am
> >very much interested to receive such mails. Whenever
> >it feels necessary, I will definately contribute.
> >
> >Pl continue to send me mails.
> >
> >Regards,
> >
> >Rajesh B. Patel
> >QC Engineer
> >Adyard Abudhabi LLC
> >
> >--- "Bathula Raghuram (Mumbai - PIPING)"
> ><R.Bathula@ticb.com> wrote:
> >
> > > No exchange of information since last 1 week, that's
> > > why you were not
> > > receiving any mails.
> > >
> > > Appreciate your concern and request members for
> > > their active
> > > participation.
> > >
> > >
> > >
> > > -----Original Message-----
> > > From: donboscomarine@vsnl.net
> > > [mailto:donboscomarine@vsnl.net]
> > >
> > > Sent: Tuesday, March 18, 2008 12:10 PM
> > > To: materials-welding@googlegroups.com
> > > Subject: Re: [MW:659] Bolt Length in ASME B31.3
> > >
> > >
> > >
> > > Dear Mr. Bathula Raghuram,
> > >
> > >
> > >
> > > We are not getting any communication since 12th
> > > March, 2008. Before
> > > that, we were witness to a very good exchange of
> > > information. Any reason
> > > for non-receipt of communication or is it just that
> > > there has been No
> > > Exchange? Will like to know the cause. We are
> > > impressed by the quality
> > > of information exchange and consider ourselves lucky
> > > to have been a
> > > memebr of this group.
> > >
> > >
> > >
> > > We will be obliged if a reply is sent ASAP.
> > >
> > >
> > >
> > > Thanks & B. Rgds.
> > >
> > >
> > >
> > > G. A. Soman
> > >
> > > Principal
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > >
> > > DON BOSCO MARITIME ACADEMY
> > >
> > > Premier Automobiles Road,
> > >
> > > Kurla West, Mumbai 400070
> > >
> > > Tel:  (022) 2504 1585 / 2018.  Fax: (022) 2504 0682
> > >
> > > Email:  donboscomarine@vsnl.net
> > >
> > > Website: www.dbma.in
> > >
> > >
> > >
> > >
> > >
> >
> >
> >
> >      ____________________________________________________________________________________
> >Be a better friend, newshound, and
> >know-it-all with Yahoo! Mobile.  Try it now.  http://mobile.yahoo.com/;_ylt=Ahu06i62sR8HDtDypao8Wcj9tAcJ
> >
> >
> >>
>
>>

PREM S NAUTIYAL
CELL : 9820313278

--~--~---------~--~----~------------~-------~--~----~
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding-unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
-~----------~----~----~----~------~----~------~--~---

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...

Maruti

Pages

Contributors

Blog Archive