Saturday, March 29, 2025

Re: [MW:35498] TEST COUPON ASME SEC IX

Yes we can use. Write in as Run sheet 16mm plate machined to 8 mm.

On Sat, 29 Mar 2025, 8:30 am Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAEabyKnxUeBK3ihVAwyXRasjZfKDKmV%3Dhw0Lx3770JCCTFmEMA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...