Re: [MW:35497] TEST COUPON ASME SEC IX

Hi elavarasan,
Can you elaborate whether you have to machine 14mm plate to 8 mm for welding, or you have to make 8mm plate instead of 14mm. 

Select the weld plate thickness based on your casting weld depth .

Incase your casting weld depth requirement is more than 2 inch better you can for 40mm plate so that you can weld as much as the depth as standard requirement, make sure you have to get approval incase you are doing major weld on the part based on customer requirement.

Regards,
Venkateshwaran 

On Sat, 29 Mar, 2025, 08:30 Elavarasan Mech, <elavarasan1861994@gmail.com> wrote:
Please clarify below 
As per ASME SEC IX can we use 14mm plate machined to 8 mm plate for WPS & WQT qualification.please guide me 
 
Regards 
ELAVARASAN 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAJ9L4ym4-UGqb6tprYjv66ifU7fan--MHmyUneojUPdVkv44Fg%40mail.gmail.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CA%2BY70uaXej5FCPuzr%2BaUD0B0jSPObOYV0E4mkCMj17SDEr0TGg%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...