Re: [MW:35449] Hot tapping between piping and pipeline

Hi

You have to follow API 1104 Annex B for qualifying the procedure

Regards
Hrishikesan

On Mon, Feb 24, 2025 at 8:24 AM ali owead <aliawead1@gmail.com> wrote:
Dear Expert
we have hot tapping 
from process piping b31.3 design 
to cross country pipeline old pipe i think api 1104 design
WPS that need to folow  api 1104 or asme b31.3.
best regard.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/ffa0c881-23d8-4b3f-96d1-7337ed4ac1e1n%40googlegroups.com.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To view this discussion visit https://groups.google.com/d/msgid/materials-welding/CAFHBd_8d%2BLmRBsV9kM6vdJHaSJ1%2BRmZO8C_45V%3D%3DOQ%3DusRqbjA%40mail.gmail.com.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...